1.1 This test method provides a quick reliable means to measure the zero-span tensile strength of a randomly oriented specimen of fibers when dry.
1.1.1 Similar procedures for determining the zero-span tensile strength of a randomly oriented specimen of fibers when wet are found in Test Method D5803.
1.2 In this test method, the fibers are tested as a handsheet produced using a standardized procedure such as TAPPI T205.
1.3 While testing is possible on finished paper materials, information on fiber quality from intermediate steps in the pulping or paper making process, or both, is frequently more useful for improving finished paper quality or improving fiber utilization of, for example, recycled fibers, or fibers subjected to new pulping, bleaching, or finishing processes.
1.4 The modifications of the procedure described in this test method required for testing finished paper is straightforward; however, testing must be done in the two principle directions of the sheet, as required in Test Method D828, since the finished paper or paperboard will generally have non-random fiber orientation, resulting in different strength properties in the two principle directions of the finished sheet.
Testing of sheets having a grammage greater than 100 g/m, which includes some paper materials described as paper and many paperboards, is difficult because of problems associated with clamping of individual fibers as the number of fibers per unit area increases.
1.5 Such modifications are not described in this test method, and if they are made, they shall be acknowledged and clearly described in the report as deviations from the standard procedure.
1.6 In addition to a measure of the dry zero-span tensile strength of the specimen of fibers, an index of the cohesiveness of fibers in the sheet is also provided by the ratio of the tensile strength determined using Test Method D828 and the tensile strength determined using this test method when all testing is done on handsheets having random fiber orientation (1).
1.7 Two instrumental approaches for accomplishing the measurement of dry tensile strength at zero-span are described.
1.8 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
1.1 This test method provides a quick reliable means to measure the zero-span tensile strength of a randomly oriented specimen of fibers when dry.
1.1.1 Similar procedures for determining the zero-span tensile strength of a randomly oriented specimen of fibers when wet are found in Test Method D5803.
1.2 In this test method, the fibers are tested as a handsheet produced using a standardized procedure such as TAPPI T205.
1.3 While testing is possible on finished paper materials, information on fiber quality from intermediate steps in the pulping or paper making process, or both, is frequently more useful for improving finished paper quality or improving fiber utilization of, for example, recycled fibers, or fibers subjected to new pulping, bleaching, or finishing processes.
1.4 The modifications of the procedure described in this test method required for testing finished paper is straightforward; however, testing must be done in the two principle directions of the sheet, as required in Test Method D828, since the finished paper or paperboard will generally have non-random fiber orientation, resulting in different strength properties in the two principle directions of the finished sheet.
Testing of sheets having a grammage greater than 100 g/m, which includes some paper materials described as paper and many paperboards, is difficult because of problems associated with clamping of individual fibers as the number of fibers per unit area increases.
1.5 Such modifications are not described in this test method, and if they are made, they shall be acknowledged and clearly described in the report as deviations from the standard procedure.
1.6 In addition to a measure of the dry zero-span tensile strength of the specimen of fibers, an index of the cohesiveness of fibers in the sheet is also provided by the ratio of the tensile strength determined using Test Method D828 and the tensile strength determined using this test method when all testing is done on handsheets having random fiber orientation (1).
1.7 Two instrumental approaches for accomplishing the measurement of dry tensile strength at zero-span are described:
1.8 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety and health practices and determine the applicability of regulatory limitations prior to use.
The zero-span tensile test measures the tensile strength at the moment of tensile failure of fibers randomly oriented in a sheet.
One important use of zero-span tensile data is to determine the maximum strength of pulp fibers when beaten under idealized laboratory conditions.
Zero-span tensile strength is an excellent measure of the βmaximum strengthβ of a pulp, and is almost completely independent of the laboratory beating procedure used.
Zero-span tensile strength, in conjunction with tensile strength as measured by Test Method D 828
Failed to load document history.
| Publish Date | Document Id | Type | View |
|---|