ASTM D885/D885M-25

Current Revision
Standard Test Methods for Tire Cords, Tire Cord Fabrics, and Industrial Filament Yarns Made from Manufactured Organic-Base Fibers

Best Price Guarantee Jun 1, 2025 English 31 Pages

Sub Total (1 Item(s)) $ 0.00
Estimated Shipping $ 0.00
Total (Pre-Tax) $ 0.00

You own the digital copy of this edition

View in Library
or
ASTM International Logo

ASTM D885/D885M-25

Standard Test Methods for Tire Cords, Tire Cord Fabrics, and Industrial Filament Yarns Made from Manufactured Organic-Base Fibers

PUBLISH DATE 2025
PAGES 31
ASTM D885/D885M-25

1.1 This standard covers the testing of industrial yarns wholly made of manufactured organic-based fibers; twisted cords made of these yarns; fabrics woven from these twisted cords; and other structures made specifically for use in manufacture of pneumatic tires.

1.1.1 These test methods can also be applicable when these yarn structures are used for reinforcing other rubber goods and fabrics made with these cords.

1.1.2 The test methods are relevant for evaluating various yarns: nylon, polyester, and rayon yarns; tire cords twisted from these yarns, and fabrics made from these yarns.

1.2 The sections on “Growth of Conditioned Yarns and Cords,” “Properties of Yarns and Cords at Elevated Temperature,” and “Properties of Wet Yarns and Cords” have been moved to Appendix X1 – Appendix X3 as non-mandatory informational items because of their very limited use by the industry and because precision and bias statements are not included.

1.3 This standard includes the following sections:

  • Adhesion of Cord to Elastomers — Section 34
  • Bibliography of Tire Cord Test Methods — Appendix X5
  • Breaking Strength (Force) of Yarns and Cords at Elevated Temperature — Section X2.3
  • Breaking Force of Conditioned Yarns and Cords — Section 16
  • Breaking Force of Oven-Dried Rayon Yarns and Cords — Section 23
  • Breaking Strength of Rayon Yarns and Cords at Specified Moisture Regain Level, Adjustment of — Section 17
  • Breaking Tenacity of Conditioned Yarns and Cords — Section 18
  • Breaking Tenacity of Oven-Dried Rayon Yarns and Cords — Section 24
  • Breaking Toughness of Yarns and Cords — Section 28
  • Commercial Mass — Section 9
  • Conditioning — Section 7
  • Contraction of Wet Yarns and Cords — Appendix X3
  • Count of Tire Cord Fabric — Section 37
  • Dip (Adhesive) Solids Pickup on Yarns and Cords — Section 33
  • Elongation at Break of Conditioned Yarns and Cords — Section 19
  • Elongation at Break of Oven-Dried Rayon Yarns and Cords — Section 25
  • Elongation of Rayon Yarns and Cords at a Specified Moisture Regain Level, Adjustment of Observed — Section 20
  • Extractable Matter in Yarns and Cords — Section 32
  • Force at Specified Elongation (FASE) of Conditioned Yarns and Cords — Section 21
  • Force-at-Specified-Elongation (FASE) of Oven-Dried Rayon Yarns and Cords — Section 26
  • Growth of Conditioned Yarns and Cords — Appendix X1
  • Identification of Fibers — Section 8
  • Keywords — Section 40
  • Linear Density — Section 11
  • Mass of per Unit Area of Tire Cord Fabric — Section 36
  • Modulus of Conditioned Yarns and Cords — Section 22
  • Moisture Regain, Actual — Section 10
  • Precision and Bias of Certain Yarn and Cord Tests — Section 39
  • Properties of Tire Cord Fabric — Sections 35 to 38
  • Sampling — Section 6
  • Shrinkage Force of Conditioned Yarns and Cords at Elevated Temperature — Section X2.5
  • Shrinkage of Conditioned Yarns and Cords at Elevated Temperature — Section X2.4
  • Significance and Use, General — Section 5
  • Significance and Use, Tensile Properties — Section 14
  • SI Calculations (examples for work-to-break, specific work-to-break, and breaking toughness) — Appendix X4
  • Stiffness of Fabric — Section 38
  • Tensile Properties of Yarns and Cords — Sections 12 to 28
  • Terminology — Section 3
  • Thickness of Cords — Section 31
  • Twist in Yarns and Cords — Section 30
  • Width of Tire Cord Fabric — Section 35
  • Work-to-Break of Yarns and Cords — Section 27

1.4 The values stated in either SI units or inch-pound units are to be regarded separately as standard. The values stated in each system may not be exact equivalents; therefore, each system shall be used independently of the other. Combining values from the two systems may result in non-conformance with the standard.

1.5 This standard does not purport to address all of the safety concerns, if any, associated with its use. It is the responsibility of the user of this standard to establish appropriate safety, health, and environmental practices and determine the applicability of regulatory limitations prior to use.

1.6 This international standard was developed in accordance with internationally recognized principles on standardization established in the Decision on Principles for the Development of International Standards, Guides and Recommendations issued by the World Trade Organization Technical Barriers to Trade (TBT) Committee.

5.1 The procedures in these test methods should be used with caution for acceptance of commercial shipments owing to the absence of factual information on the between-laboratory precision of many of the test procedures included in these test methods.

It is recommended that any program of acceptance testing be preceded by an interlaboratory check in the laboratory of the purchaser and the laboratory of the supplier on replicate specimens of the materials to be tested for each property (or properties) to be evaluated.

5.1.1 If there are differences of practical significance between reported test results for two laboratories (or more), comparative tests should be performed to determine if there is a statistical bias between them, using competent statistical assistance.

  • As a minimum, test samples should be used that are as homogeneous as possible, that are drawn from the material from which the disparate test results were obtained, and that are randomly assigned in equal numbers to each laboratory for testing.
  • Other materials with established test values may be used for this purpose.
  • The test results from the two laboratories should be compared using a statistical test for unpaired data, at a probability level chosen prior to the testing series.
  • If a bias is found, either its cause must be found and corrected, or future test results must be adjusted in consideration of the known bias.

5.2 The significance and use of particular properties are discussed in the appropriate sections of specific test methods.

Loading...

Failed to load document history.

Publish Date Document Id Type View