Logo
Login Sign Up
Current Revision

BSI BS 8701:2016

Full ring ovalization test for determining the susceptibility to cracking of linepipe steels in sour service. Test method
Best Price Guarantee
Instant

$399.79

2-5 Days

$399.79

SAVE 10%

$719.62


Sub Total (1 Item(s))

$ 0.00

Estimated Shipping

$ 0.00

Total (Pre-Tax)

$ 0.00


View in Library
or
British Standards Institution Logo

BSI BS 8701:2016

Full ring ovalization test for determining the susceptibility to cracking of linepipe steels in sour service. Test method

PUBLISH DATE 2016
PAGES 56
BSI BS 8701:2016

This British Standard gives a method for determining the susceptibility to cracking of steel pipes in sour service.

This British Standard utilizes a tubular specimen comprising a full circumferential ring. The test method applies to any pipe with or without seam (longitudinal or spiral) or girth weld (with or without filler).

NOTE 1 The specimen is usually a pipe but can also consist of flange neck or section of a bend, or other tubular component or a combination of the above.

This British Standard provides guidance on determination of specimen size to ensure it retains residual stresses from manufacture and welding.

NOTE 2 See Clause 7 for specimen sizes.

The method utilizes ovalization to simulate hoop stress, using mechanical loading on a tubular form. The specimen is subjected to single sided exposure to the sour test environment.

NOTE 3 The test also allows measurement of hydrogen permeation rates which can provide useful information, such as highlighting the effects of galvanic coupling between materials of apparent compatibility.

SDO BSI: British Standards Institution
Document Number 8701
Publication Date June 30, 2016
Language en - English
Page Count
Revision Level
Supercedes
Committee PSE/17
Loading...

Failed to load document history.