Fine ceramics (advanced ceramics, advanced technical ceramics). Mechanical properties of ceramic composites at high temperature. Determination of stress-rupture time diagram under constant tensile loading
This document specifies the conditions for determination of the stress-rupture time diagram of continuous fibre-reinforced ceramic matrix composites (including carbon fibre-reinforced carbon matrix composite) at high temperature in air, vacuum and inert gas atmospheres under constant tensile loading.
This document applies to all ceramic matrix composites with continuous fibre reinforcement: unidirectional (1D), bidirectional (2D) and tridirectional (xD, with 2Β <Β xΒ β€Β 3), loaded along one principal axis of reinforcement.
NOTEΒ 1: In most cases, ceramic matrix composites to be used at high temperature in air are coated with an antioxidation coating.
NOTEΒ 2: Since the main purpose of the test is to obtain the stress-rupture time data, the deformation measurement is not mandatory.
Failed to load document history.
| Publish Date | Document Id | Type | View |
|---|