A collection of featured documents from our library that are popular among our users or otherwise noteworthy.
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings and Stock for Forging 41.5Ni - 16Cr - 37Fe - 2.9Cb - 1.8Ti Consumable Electrode or Vacuum Induction Melted 1750 °F (954 °C) Solution, Stabilization, and Precipitation Heat Treated
Nickel Alloy, Corrosion and Heat Resistant, Forgings 57Ni - 19.5Cr - 13.5Co - 4.6Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, and Rings 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.006B - 0.05Zr Consumable Electrode or Vacuum Induction Melted 1825 to 1900 °F Solution Heat Treated
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging Stock 57Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B Consumable Electrode Remelted or Vacuum Induction Melted 1825 to 1900 °F (996 to 1038 °C) Solution, Stabilization, and Precipitation Heat Treated
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Rings, Forging, Flash-Welded Rings and Heading Stock 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B (Waspaloy) Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated
Nickel Alloy, Corrosion- and Heat-Resistant, Bars and Forgings, 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B, Consumable Electrode or Vacuum Induction Melted, 1975 °F (1079 °C) Solution Heat Treated, Stabilized, and Precipitation Heat Treated
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings 53Ni - 19Cr - 11Co - 9.8Mo - 3.2Ti - 1.6Al - 0.006B Vacuum Melted, Solution Heat Treated Precipitation Hardenable
Steel Bars, Wire, Forgings and Forging Stock, Mechanical Tubing, Rings, and Extrusions, Corrosion-Resistant 11.8Cr - 2.5Ni - 1.8Mo - 0.33V (0.08 - 0.15C) Annealed, Vacuum Arc or Electroslag Remelted
Steel, Corrosion- and Heat-Resistant, Bars and Wire 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V 1800 °F (982 °C) Solution Heat Treated and Work-Strengthened Consumable Electrode Remelted 200 ksi (1379 MPa) Tensile Strength Capability
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted, 1800 °F (982 °C) Solution Heat Treated Precipitation Hardenable
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted 1800 °F (982 °C) Solution and Precipitation Heat Treated
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (Alloy A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution Heat Treated
STEEL BARS, FORGINGS, TUBING, AND RINGS, CORROSION AND HEAT RESISTANT 15Cr - 26Ni - 1.3Mo - 2.1Ti - 0.30V 1800° F (982.2° C) Solution and Precipitation Heat Treated
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted 1650 °F (899 °C) Solution and Precipitation Heat Treated
Steel, Corrosion- and Heat-Resistant, Bars, Forgings and Forging Stock, 15.5Cr - 4.5Ni - 2.9Mo - 0.10N (AM 355®), Consumable Electrode Remelted, Solution Heat Treated, Subzero Cooled, Equalized, and Over-Tempered
Alloy, Corrosion- and Heat-Resistant, Bars and Forgings 15Cr - 45Ni - 4.1Mo - 4.1W - 3.0Ti - 1.0Al - 31Fe (D979) Consumable Electrode Vacuum Melted Solution and Precipitation Heat Treated
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, and Rings 72Ni - 15.5Cr - 0.95Cb(Nb) - 2.5Ti - 0.70Al - 7.0Fe 1800 °F (982 °C) Solution Heat Treated, Precipitation Hardenable
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Forging Stock and Mechanical Tubing 14.5Cr - 4.0Mo - 1.2V (1.10-1.20C) Premium Quality for Bearing Applications, Double Vacuum Melted
Alloy Bars, Forgings, and Rings, Corrosion and Heat Resistant Nickel Base - 15.5Cr - 16Mo - 3.8W - 5.5Fe Solution Heat Treated
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Forging, Ring, and Heading Stock 47.5Ni - 22Cr - 1.5Co - 9.0Mo - 0.60W - 18.5Fe (Alloy X) Solution Heat Treated
Cobalt Alloy, Corrosion- and Heat-Resistant, Bars, Forging Stock, Forgings, and Rings, 52Co - 20Cr - 10Ni - 15W (L-605)
Steel, Corrosion-Resistant Bars, Forgings, Mechanical Tubing, and Rings and Forging Stock 15Cr - 6.5Ni - 0.75Mo - 0.50Cb (Nb) - 1.5Cu Solution Heat Treated
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Extrusions, Rings, and Forging Stock 5.0Mn - 22Cr - 12.5Ni - 2.2Mo - 0.20Cb - 0.30N - 0.20V (SAE XM-19), Solution Heat Treated
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings or Rings 15Cr - 6.5Ni - 0.75Mo - 0.30Cb (Nb) - 1.5Cu Consumable Electrode Remelted, Solution Heat Treated, Precipitation Hardenable
Steel, Corrosion- and Heat-Resistant, Welding Wire, 12.5Cr (SAE 410)