| SAE |
SAE AMS5773 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings or Rings 15Cr - 6.5Ni - 0.75Mo - 0.30Cb (Nb) - 1.5Cu Consumable Electrode Remelted, Solution Heat Treated, Precipitation Hardenable
|
|
| SAE |
SAE AMS5612 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Stock for Forging and Flash-Welded Rings, 12Cr (410), Aircraft Quality, Ferrite Controlled, Annealed
|
|
| SAE |
SAE AMS5647 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Forging Stock 19Cr - 9.5Ni Solution Heat Treated
|
|
| SAE |
SAE AMS5895 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging Stock, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286), Consumable Electrode Melted, 1750 °F (954 °C) Solution Heat Treated, Welding Grade, Precipitation Hardenable
|
|
| SAE |
SAE AMS5769 |
Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings, 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0(Cb+Ta) - 0.15N - 32Fe (N-155), Solution Heat Treated
|
|
| SAE |
SAE AMS5926 |
Steel, Corrosion-Resistant, Bars, Wire, Mechanical Tubing, Forgings and Forging Stock 15.5Cr - 1.5Si - 0.3Mo - 0.1N (0.45 - 0.60C) for Bearing Applications
|
|
| SAE |
SAE AMS5771 |
Nickel Alloy, Corrosion and Heat-Resistant, Bars, Forgings, Rings, and Stock for Forgings and Rings 74Ni - 7.0Cr - 16.5Mo (Hastelloy® N) Solution Heat Treated
|
|
| SAE |
SAE AMS5768 |
Alloy, Corrosion and Heat-Resistant, Bars, Wire, Forgings, Rings and Stock for Forgings, Rings and Heading 21Cr - 20Ni - 20Co - 3.0Mo - 2.5W - 1.0Cb - 0.15N - 31Fe Solution and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5572 |
Steel, Corrosion and Heat-Resistant, Seamless Tubing, 25Cr - 20Ni (SAE 30310S), Solution Heat Treated
|
|
| SAE |
SAE AMS5577 |
Steel, Corrosion and Heat Resistant, Welded Tubing 25Cr - 20Ni (310) Solution Heat Treated
|
|
| SAE |
SAE AMS5719 |
Steel Bars, Wire, Forgings and Forging Stock, Mechanical Tubing, Rings, and Extrusions, Corrosion-Resistant 11.8Cr - 2.5Ni - 1.8Mo - 0.33V (0.08 - 0.15C) Annealed, Vacuum Arc or Electroslag Remelted
|
|
| SAE |
SAE AMS5731 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted, 1800 °F (982 °C) Solution Heat Treated Precipitation Hardenable
|
|
| SAE |
SAE AMS5654 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical
Tubing, Rings and Forging Stock 18Cr - 11Ni - 0.60Cb (Nb) (347) Premium Aircraft
Quality, Consumable Electrode Melted Solution Heat Treated
|
|
| SAE |
SAE AMS5656 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Extrusions, Rings and Forging Stock 9.0Mn - 20Cr - 6.5Ni - 0.27N Solution Heat Treated
|
|
| SAE |
SAE AMS5734 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Stock for Forging and Heading, 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (Alloy A286), Consumable Electrode Remelted, 1650 °F (899 °C) Solution Heat Treated
|
|
| SAE |
SAE AMS5639 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging and Ring Stock 19Cr - 10Ni Solution Heat Treated
|
|
| SAE |
SAE AMS5708 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Rings, Forging, Flash-Welded Rings and Heading Stock 58Ni - 19.5Cr - 13.5Co - 4.3Mo - 3.0Ti - 1.4Al - 0.05Zr - 0.006B (Waspaloy) Consumable Electrode or Vacuum Induction Melted 1975 °F (1079 °C) Solution Heat Treated
|
|
| SAE |
SAE AMS5653 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forging and Rings 17Cr - 12Ni - 2.5Mo (0.030 Max C) (316L), Solution Heat Treated
|
|
| SAE |
SAE AMS5628 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing and Forging Stock, 16Cr - 2.5Ni (SAE 51431), Aircraft Quality
|
|
| SAE |
SAE AMS5645 |
Steel, Corrosion and Heat Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings and Forging Stock 18Cr - 10Ni - 0.40Ti (321) Solution Heat Treated
|
|
| SAE |
SAE AMS5854 |
Nickel Alloy, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Rings, Extrusions, and Stock for Forgings and Rings, 61Ni - 20.5Cr - 8.5Mo - 3.4Cb(Nb) - 1.3Ti - 5.0Fe (Alloy 716), Consumable Electrode or Vacuum Induction Melted, Solution Heat Treated
|
|
| SAE |
SAE AMS5643 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Mechanical Tubing, and Rings 16Cr - 4.0Ni - 0.30Cb (Nb) - 4.0Cu Solution Heat Treated, Precipitation Hardenable
|
|
| SAE |
SAE AMS5661 |
Nickel-Iron Alloy, Corrosion- and Heat-Resistant, Bars, Forgings, Rings and Stock for Forging or Flash-Welded Rings 42.5Ni - 12.5Cr - 5.8Mo - 2.9Ti - 0.015B - 35Fe (Alloy 901) Consumable Electrode Remelted or Vacuum Induction Melted Solution Heat Treated, Stabilized, and Precipitation Heat Treated
|
|
| SAE |
SAE AMS5749 |
Steel, Corrosion-Resistant, Bars, Wire, Forgings, Forging Stock and Mechanical Tubing 14.5Cr - 4.0Mo - 1.2V (1.10-1.20C) Premium Quality for Bearing Applications, Double Vacuum Melted
|
|
| SAE |
SAE AMS5732 |
Steel, Corrosion- and Heat-Resistant, Bars, Wire, Forgings, Mechanical Tubing, Rings, and Stock for Forgings, Rings, or Heading 15Cr - 25.5Ni - 1.2Mo - 2.1Ti - 0.006B - 0.30V (A286) Consumable Electrode Remelted 1800 °F (982 °C) Solution and Precipitation Heat Treated
|
|